Equal material : Hastelloy C
NS3303/ NS333 which is on the basis of Hastelloy alloy B adding elements of Cr, w, Ni - Cr alloy and N i.M o is compatible and optimization, in the oxidizing and reducing medium has good corrosion resistance and resistance to local corrosion, resistance to chloride stress corrosion cracking and pitting corrosion of sea water. NS3303/ NS333there are some serious drawbacks, in demanding oxidation medium, the alloy of chromium content is not enough to keep its passivation state and showed high uniform corrosion rate; More applications obstacle is the welding heat affected zone in many oxidizing, low pH, halide environment is sensitive to intergranular corrosion. Many applications require made of NS3303/ NS333alloy container must after solid solution treatment after welding eliminate segregation of heat affected zone, which seriously limits the application of this alloy.
NS3303/ NS333alloy steel Chemical composition
| Ni | Cr | Mo | Fe | W | Co | C | Mn | Si | V | P | S | |
|
Min
|
Balance
|
14.5
|
15
|
4
|
3
|
|
|
|
|
|
|
|
|
Max
|
16.5
|
17
|
7
|
4.5
|
2.5
|
0.08
|
1
|
1
|
0.35
|
0.04
|
0.03
|
NS3303/ NS333Physical properties:
NS3303/ NS333Density: 8.94 g/cm3
NS3303/ NS333Melting point: 1350 degree
NS3303/ NS333Alloy mechanical properties at room temperature:
|
Alloy state
|
Tensile strength MPa
|
Yield strength MPa
|
elongation A5 %
|
|
NS3303/ NS333alloy bar
|
690
|
315
|
30
|
|
690
|
315
|
30
|
|
|
NS3303/ NS333alloy colled rolled sheet
|
690
|
285
|
40
|
|
NS3303/ NS333alloy strip
|
690
|
315
|
30
|
- Nickle alloys & Super alloys
- Stainless steel & Heat resistant steel
- Carbon steel
- Low alloy high strength steel
- High strength steel
- Boiler steel plate
- Shipbuilding steel plate
- Bridge structural steel
- Weathering steel
- Wear resistant steel
- Pipeline steel
- High carbon steel
- Alloy steel
- CQ/DQ/DDQ/CSS/HSS Grade steel
- Hot rolled steel coil
- Cold rolled steel coil
- Pickled & oiled steel coil
- Electrical steel
- Galvanized and prepainted steel
- Shipbuilding angle steel bar
- Shipbuilding bulb flat bar
- Shipbuilding L shape bars