UNSS66286 is A Fe-ni- cr 15 25 based high temperature alloy, molybdenum, titanium, aluminum, vanadium and trace boron composite reinforcement.Under 650 degree has high yield strength and lasting and creep strength, and has good processing plastic and satisfactory welding performance.Suitable for manufacturing in the long-term work of aircraft engine under 650 degree high temperature bearing parts, such as turbine disc, press plate, the rotor blades and fasteners, etc.Can produce all kinds of deformation in the shape of the alloy products, such as plate, forgings, plate, bar, wire and circular pieces, etc.High-quality UNSS66286 alloy, which is on the basis of Incoloy A - 286 alloy development,aslong as is to improve the alloy purity, gas content, control the content of low melting point elements, and adjust the system of heat treatment, so that the alloy heat intensity and the long-term use of performance improvement.
1. UNSS66286 steel equal material : A286,UNSS66286,P.Q.A286, Incoloy A - 286
2. UNSS66286alloy chemical composition %
|
C
|
Cr
|
Ni
|
Mo
|
Ti
|
V
|
B
|
Mn
|
Al
|
Si
|
P
|
S
|
FE
|
|
≤0.08
|
13.5- 16.0
|
24.0- 27.0
|
1.00- 1.50
|
1.75- 2.30
|
0.10- 0.50
|
0.001-0.010
|
1.00- 2.00
|
≤0.04
|
≤1.00
|
≤0.030
|
≤0.020
|
remaining
|
Note:UNSS66286Cold drawing steel rods, UNSS66286steel disc and UNSS66286steel ring standard rules (Ti)1.80%-2.35%。
UNSS66286Hot rolled steel sheet and UNSS66286cold rolled steel sheet standard requirements (B)0.003%-0.010%, (Mn)≤2.00%, (P)≤0.020%, (S)≤0.015%。
UNSS66286Cold drawn wire standard request (Al)≤0.35%, (Ti)1.75%-2.35%, (Si)0.40%-1.00%, (P)≤0.020%, (S)≤0.015%。
UNSS66286Cold heading with silk material standards request: (Ti)1.75%-2.35%, (Si)0.40%-1.00%, (P)≤0.025%, (S)≤0.020%。
UNSS66286Hot rolled and forged bar standard request (Cu)≤0.25%.
High-quality Incoloy A - 286 alloy chemical composition %
|
C
|
Cr
|
Ni
|
Mo
|
Ti
|
Fe
|
V
|
B
|
Mn
|
Al
|
Si
|
P
|
S
|
|||||||||
|
≤
|
|||||||||||||||||||||
|
≤0.08
|
13.50-16.00
|
24.00-27.00
|
1.00- 1.50
|
1.90- 2.35
|
remaining
|
0.10-0.50
|
0.003-0.010
|
0.35
|
0.35
|
0.35
|
0.015
|
0.002
|
|||||||||
|
Ca
|
Mg
|
Cu
|
Sn
|
Pb
|
Se
|
Ag
|
Te
|
Tl
|
Bi
|
N
|
O
|
||||||||||
|
≤
|
|||||||||||||||||||||
|
0.005
|
0.005
|
0.30
|
0.0050
|
0.0005
|
0.0003
|
0.0005
|
0.00005
|
0.0001
|
0.00003
|
0.0100
|
0.0050
|
||||||||||
3. UNSS66286Heat treatment system are shown in the following table. Quality Incoloy A - 286 heat treatment is at 900 degree plus or minus 10 degree, 1 ~ 2 h, oil cooled to + 750 degree + 10 degree, 16 h, air cooling.
|
Product
|
Heat treatment system
|
|
UNSS66286 Rod bar, disc
|
980-1000 degree,1-2h, Oil cooling+700-720 degree, 12-16h, Air cooling
|
|
UNSS66286 Hot rolled / cold rolled plates
|
980-1000 degree, Air cooling+700-720degree, 12-16h, Air cooling
|
|
UNSS66286 Cold drawn rod
|
980-1000 degree,1-2h,Oil cooling+700-720℃,16h, Air cooling
|
|
UNSS66286 Ring
|
980-990 degree 1-2h, Oil cooling+700-720degree, 16h, Air cooling
|
|
UNSS66286 cold drawing wire
|
980-1000degree, Water cooling or Oil cooling+700-720 degree,16h, Air cooling
|
- Nickle alloys & Super alloys
- Stainless steel & Heat resistant steel
- Carbon steel
- Low alloy high strength steel
- High strength steel
- Boiler steel plate
- Shipbuilding steel plate
- Bridge structural steel
- Weathering steel
- Wear resistant steel
- Pipeline steel
- High carbon steel
- Alloy steel
- CQ/DQ/DDQ/CSS/HSS Grade steel
- Hot rolled steel coil
- Cold rolled steel coil
- Pickled & oiled steel coil
- Electrical steel
- Galvanized and prepainted steel
- Shipbuilding angle steel bar
- Shipbuilding bulb flat bar
- Shipbuilding L shape bars