ZbNCT25iron-based wrought superalloy
ZbNCT25 is A Fe - ni - cr 15 25 based high temperature alloy, molybdenum, titanium, aluminum, vanadium and trace boron composite reinforcement.Under 650 degree has high yield strength and lasting and creep strength, and has good processing plastic and satisfactory welding performance.Suitable for manufacturing in the long term work of aircraft engine under 650 degree high temperature bearing parts, such as turbine disc, press plate, the rotor blades and fasteners, etc.Can produce all kinds of deformation in the shape of the alloy products, such as plate, forgings, plate, bar, wire and circular pieces, etc.
High-quality ZbNCT25 alloy, which is on the basis of ZbNCT25 alloy development, as long as is to improve the alloy purity, gas content, control the
content of low melting point elements, and adjust the system of heat treatment, so that the alloy heat intensity and the long-term use of performance improvement.
1.ZbNCT25 steel equal material : A286,UNSS66286,P.Q.A286, Incoloy A - 286
2.ZbNCT25 alloy chemical composition %
| C | Cr | Ni | Mo | Ti | V | B | Mn | Al | Si | P | S | FE |
| ≤0.08 | 13.5- 16.0 | 24.0- 27.0 | 1.00- 1.50 | 1.75- 2.30 | 0.10- 0.50 | 0.001-0.010 | 1.00- 2.00 | ≤0.04 | ≤1.00 | ≤0.030 | ≤0.020 | remaining |
ZbNCT25Hot rolled steel sheet and ZbNCT25cold rolled steel sheet standard requirements (B)0.003%-0.010%, (Mn)≤2.00%, (P)≤0.020%, (S)≤0.015%。
ZbNCT25Cold drawn wire standard request (Al)≤0.35%, (Ti)1.75%-2.35%, (Si)0.40%-1.00%, (P)≤0.020%, (S)≤0.015%。
ZbNCT25Cold heading with silk material standards request: (Ti)1.75%-2.35%, (Si)0.40%-1.00%, (P)≤0.025%, (S)≤0.020%。
ZbNCT25Hot rolled and forged bar standard request (Cu)≤0.25%。
High-quality Incoloy A - 286 alloy chemical composition %
| C | Cr | Ni | Mo | Ti | Fe | V | B | Mn | Al | Si | P | S | |||||||||
| ≤ | |||||||||||||||||||||
| ≤0.08 | 13.50-16.00 | 24.00-27.00 | 1.00- 1.50 | 1.90- 2.35 | remaining | 0.10-0.50 | 0.003-0.010 | 0.35 | 0.35 | 0.35 | 0.015 | 0.002 | |||||||||
| Ca | Mg | Cu | Sn | Pb | Se | Ag | Te | Tl | Bi | N | O | ||||||||||
| ≤ | |||||||||||||||||||||
| 0.005 | 0.005 | 0.30 | 0.0050 | 0.0005 | 0.0003 | 0.0005 | 0.00005 | 0.0001 | 0.00003 | 0.0100 | 0.0050 | ||||||||||
3. ZbNCT25Heat treatment system are shown in the following table. Quality Incoloy A - 286 heat treatment is at 900 degree plus or minus 10 degree, 1 ~ 2 h, oil cooled to + 750 degree + 10 degree, 16 h, air cooling.< br>
| Product | Heat treatment system |
| ZbNCT25 Rod bar, disc | 980-1000 degree,1-2h, Oil cooling+700-720 degree, 12-16h, Air cooling |
| ZbNCT25 Hot rolled / cold rolled plates | 980-1000 degree, Air cooling+700-720degree, 12-16h, Air cooling |
| ZbNCT25 Cold drawn rod | 980-1000 degree,1-2h,Oil cooling+700-720℃,16h, Air cooling |
| ZbNCT25 Ring | 980-990 degree 1-2h, Oil cooling+700-720degree, 16h, Air cooling |
| ZbNCT25 cold drawing wire | 980-1000degree, Water cooling or Oil cooling+700-720 degree,16h, Air cooling |
- Nickle alloys & Super alloys
- Stainless steel & Heat resistant steel
- Carbon steel
- Low alloy high strength steel
- High strength steel
- Boiler steel plate
- Shipbuilding steel plate
- Bridge structural steel
- Weathering steel
- Wear resistant steel
- Pipeline steel
- High carbon steel
- Alloy steel
- CQ/DQ/DDQ/CSS/HSS Grade steel
- Hot rolled steel coil
- Cold rolled steel coil
- Pickled & oiled steel coil
- Electrical steel
- Galvanized and prepainted steel
- Shipbuilding angle steel bar
- Shipbuilding bulb flat bar
- Shipbuilding L shape bars