NiCr15Fe7TiAl Wrought nickel-base superalloy
NiCr15Fe7TiAl Alloy steel is mainly by γ [Ni3 (Al, Ti, Nb)] phase of nickel base superalloy aging strengthening, has good corrosion resistance and oxidation resistance at 980 degree, 800 degree with higher intensity, 540 degree with relaxation has good performance, but also has the forming and welding performance good. This alloy is mainly used in the manufacture of aero engine under 800 degree and requirements and high strength corrosion resistant ring parts, structural parts and bolts and other components, in 540 degree work with medium or low stress and resistance to planar spring relaxation and spiral spring. Also can be used in the manufacture of gas turbine blades. Can supply a variety of sheet, strip, bars, forgings, ring, wires and tubes.
1. NiCr15Fe7TiAl Wrounght nickel-base superalloy equal material :GH145 / GH4145, NC15FeTNbA, NCF750
2. NiCr15Fe7TiAl Alloy steel Chemical composition
| C | Cr | Ni+Co | Al | Ti | Fe | Nb+Ta | Co | Mn | Si | S | Cu | P |
| ≤ | ||||||||||||
| ≤0.08 | 14.0-17.0 | ≥70.0 | 0.40-1.00 | 2.25-2.75 | 5.00-9.00 | 0.70-1.20 | 1.00 | 1.00 | 0.50 | 0.010 | 0.50 | 0.015 |
3. NiCr15Fe7TiAl Alloy steel physical properties
NiCr15Fe7TiAl Alloy steel The melting temperature range 1395-1425 degree.
NiCr15Fe7TiAl Alloy steel Density : 8.25g/cm3
4. NiCr15Fe7TiAl alloy steel Mechanical properties
| Product | Tensile strength /MPa | Yield strength MPa | Elongation /% | HRC |
| NiCr15Fe7TiAl Alloy steel Strip | ≤930 | - | ≥18 | - |
| ≥1105 | - | ≥12 | ≥30 | |
| NiCr15Fe7TiAl Alloy cold rolled steel sheet | ≤930 | ≤515 | ≥30 | - |
| ≤930 | ≤515 | ≥35 | - | |
| NiCr15Fe7TiAl Alloy hot rooled steel plate | ≥1170 | ≥795 | ≥18 | ≥32 |
| NiCr15Fe7TiAl Alloy steel tube | ≤965 | ≤550 | ≥35 | - |
| ≥1170 | ≥790 | ≥15 | - |
- Nickle alloys & Super alloys
- Stainless steel & Heat resistant steel
- Carbon steel
- Low alloy high strength steel
- High strength steel
- Boiler steel plate
- Shipbuilding steel plate
- Bridge structural steel
- Weathering steel
- Wear resistant steel
- Pipeline steel
- High carbon steel
- Alloy steel
- CQ/DQ/DDQ/CSS/HSS Grade steel
- Hot rolled steel coil
- Cold rolled steel coil
- Pickled & oiled steel coil
- Electrical steel
- Galvanized and prepainted steel
- Shipbuilding angle steel bar
- Shipbuilding bulb flat bar
- Shipbuilding L shape bars