NiCr22FeMo is a kind nickel base super alloy with Cr and Mo solid solution having a high iron content, strengthening, has good anti raising and corrosion resistance, moderate endurance and creep strength at 900 degree, cold, hot workability and good welding performance. The combustion chamber components used in the manufacture of aircraft engines and other high temperature components, long-term use under 900 degree, short-time working temperature can reach 1080 degree. The main varieties of supply of sheet, strip, pipe, bars, forgings, rings and precision casting.
1. NiCr22FeMo alloy equal material:
GH3536/GH536/GH22/GH334/GH739/SG-5(China),UNS NO6002, NC22FeD(France), Hastelloy X, Nimonic PE13(British)
2.NiCr22FeMo Wrought nickel-base superalloy Chemical composition
|
C
|
Cr
|
Ni
|
Co
|
W
|
Mo
|
Al
|
Ti
|
Fe
|
B
|
Cu
|
Mn
|
Si
|
P
|
S
|
|
No more than
|
||||||||||||||
|
0.05- 0.15
|
20.5- 23.0
|
balance
|
0.50- 2.50
|
0.20- 1.00
|
8.0- 10.0
|
≤0.50
|
≤0.15
|
17.0- 20.0
|
0.010
|
0.50
|
1.00
|
1.00
|
0.025
|
0.015
|
3. NiCr22FeMo material Heat treatment system
Sheet and pipe: 1130 - 1170 degree, fast air cooling or water cooling;
Bar and ring pieces : 1175±15 degree , air cooling or faster cooling;
Strip: 1065 - 1105 degree , fast cooling.
4. NiCr22FeMo alloy steel supply specifications
Sheet : thickness 0.5 ~ 4.0 mm
Strip : thickness 0.05 ~ 0.8 mm
Pipe: 4 - 20 mm outside diameter, wall thickness of 1.0 ~ 2.0 mm
Wire: diameter 0.2 ~ 10.0 mm
Bar: diameter 300 mm or less
Ring: all kinds of diameter and wall thickness and the precision casting of different shapes and sizes
5. NiCr22FeMo alloy steel supply Condition:
Sheet, strip and tubes : after solid solution treatment and acid cleaning
Strip : in cold rolling state
Welding wire: before hard and half hard, solid fusion and pickling, light solid solution treatment status in coil delivery, also can direct the delivery
Bar and annular parts: without heat treatment delivery
Precision casting : supply in casting state
6. NiCr22FeMo alloy steel application and special requirements
NiCr22FeMo alloy mainly used in the manufacture of hot end of combustion chamber parts and other components, and honeycomb structure, etc. Alloy at high temperature after long-term use of certain age hardening phenomenon.
7. NiCr22FeMo physical properties
NiCr22FeMo Melting temperature range: 1295-1381 degree.
NiCr22FeMo Density: 8.28g/cm3.
8. NiCr22FeMo Mechanical property:
|
Product
|
Room temperature
|
815 degree Persistent property
|
Other properties
|
||||
|
Yield strength /MPa
|
Tensile strength /MPa
|
elongation δ5/%
|
σ/MPa
|
t/h
|
δ5/%
|
||
|
no less than
|
|||||||
|
Cold rolled sheet Cold rolled strip Cold drawn pipe bar Ring a casting
|
310 310 310 275 275 200
|
725 760 690 690 690 380
|
35 30 25 30 30 10
|
110 - - 105 105 -
|
24 - - 24 24 -
|
8.0 - - 10.0 10.0 -
|
bending 180° bending 180° Hydraulic, flaring HBS≤241 HBS≤241 HBS≤96
|
- Nickle alloys & Super alloys
- Stainless steel & Heat resistant steel
- Carbon steel
- Low alloy high strength steel
- High strength steel
- Boiler steel plate
- Shipbuilding steel plate
- Bridge structural steel
- Weathering steel
- Wear resistant steel
- Pipeline steel
- High carbon steel
- Alloy steel
- CQ/DQ/DDQ/CSS/HSS Grade steel
- Hot rolled steel coil
- Cold rolled steel coil