N06600 The early development of Ni Cr Fe based solid solution strengthened alloys, has good resistance to high temperature corrosion and oxidation resistance, hot and cold processing quality and welding performance is satisfactory, heat resistance and high plasticity at 700 degree. Alloy can be enhanced by cold working, can also be connected with the resistance welding, welding or soldering solution, which can supply cold rolled sheet, hot-rolled plate, strip, wire, bar, pie, the ring blank, forging ring, suitable for making under low load of antioxidant components in 1100 degree .
N06600 equal material : Inconel600
N06600 chemical composition %
C |
Cr |
Ni+Co |
Al |
Ti |
Fe |
Nb+Ta |
Mn |
Si |
P |
S |
Cu |
≤0.15 |
14.0-17.0 |
≥72 |
≤0.35 |
≤0.50 |
6.00~10.00 |
≤1.00 |
≤1.00 |
≤0.50 |
≤0.040 |
≤0.015 |
≤0.50 |
Heat treatment
Product |
Heat treatment system |
N06600 steel plate |
1010-1050 degree,3-5 min/mm, Air cooling |
N06600 steel strip |
1010±10 degree, Air cooling |
N06600 wire |
1065±10 degree, Air cooling |
N06600 Ring and Rod |
1010±10 degree, Air cooling |
(1) non vacuum induction melting and electroslag remelting;
(2) electric arc furnace melting and electroslag remelting;
(3) the vacuum melting.
5.N06600 The physical and chemical properties.
N06600 steel melting temperature 1370-1430 degree
N06600 density : 8.43g/cm3
N06600 mechanical property
Product |
θ/℃ |
Tensile property |
HBS |
Bending test |
|||
σb/MPa |
σP0.2/MPa |
δ5/% |
φ/% |
||||
N06600 steel bar |
20 |
≥585 |
≥240 |
≥30 |
- |
134-217 |
- |
N06600 steel ring, Cake or loop |
20 |
≥520 |
≥205 |
≥35 |
- |
≥187 |
- |
N06600 steel Hot rolled plate |
20 |
≥550 |
≥240 |
≥35 |
≥40 |
- |
- |
900 |
≥95 |
≥45 |
≥40 |
≥50 |
- |
- |
|
N06600 steel Cold rolled plate |
20 |
≥550 |
≥240 |
≥30 |
- |
- |
|
900 |
≥90 |
≥40 |
≥60 |
- |
- |
- |
|
Cold rolled plate |
20 |
≥550 |
≥200 |
≥30 |
- |
- |
test |
N06600 steel strip |
20 |
≥550 |
≥240 |
≥30 |
- |
- |
|
N06600 alloy steel forming properties : has good processing performance, ingot forging heating temperature 1110 -1140 degree; the final forging temperature less than 950 degree, slab rolling heating temperature 1130 - 1170 degree, finishing the heating temperature is 1090 - 1130 degree. The finished product solid solution treatment temperature of 1010 -1050 degree.
N06600 alloy steel Good welding performance properties : welding, connection available electric arc welding, argon arc welding, resistance welding and brazing and other methods, large or complex welding pieces of the structure in the welding should be at 870 degree for 1h, to eliminate the welding stress.
N06600 alloy steel Heat treatment process : should be carried out according to the heat treatment system of the corresponding material standard. Annealed sheet and strip parts should be carried out in a protective atmosphere.
Related Link:Inconel 600,Inconel 601,Inconel 617,Inconel 625,Inconel 690,Inconel 718,Inconel X750,Nickel alloys and super alloys
- Nickle alloys & Super alloys
- Stainless steel & Heat resistant steel
- Carbon steel
- Low alloy high strength steel
- High strength steel
- Boiler steel plate
- Shipbuilding steel plate
- Bridge structural steel
- Weathering steel
- Wear resistant steel
- Pipeline steel
- High carbon steel
- Alloy steel
- CQ/DQ/DDQ/CSS/HSS Grade steel
- Hot rolled steel coil
- Cold rolled steel coil
- Pickled & oiled steel coil
- Electrical steel
- Galvanized and prepainted steel
- Shipbuilding angle steel bar
- Shipbuilding bulb flat bar
- Shipbuilding L shape bars