Inconel X-750 Wrought nickel-base superalloy

Inconel X-750 Alloy steelis mainly by γ [Ni3 (Al, Ti, Nb)] phase of nickel base superalloy aging strengthening,has good corrosion resistance and oxidation resistance at 980 degree, 800 degree with higher intensity, 540 degree with relaxation has good performance, but also has the forming and welding performance good. This alloy is mainly used in the manufacture of aero engine under 800 degree and requirements and high strength corrosion resistant ring parts, structural parts and bolts and other components, in 540 degree work with medium or low stress and resistance to planar spring relaxation and spiral spring. Also can be used in the manufacture of gas turbine blades. Can supply a variety of sheet, strip, bars, forgings, ring, wires and tubes.
1. Inconel X-750 Wrounght nickel-base superalloy equal material :GH145 / GH4145, NiCr15Fe7TiAl, NC15FeTNbA, NCF750
2. Inconel X-750 Alloy steel Chemical composition
|
C
|
Cr
|
Ni+Co
|
Al
|
Ti
|
Fe
|
Nb+Ta
|
Co
|
Mn
|
Si
|
S
|
Cu
|
P
|
|
≤
|
||||||||||||
|
≤0.08
|
14.0-17.0
|
≥70.0
|
0.40-1.00
|
2.25-2.75
|
5.00-9.00
|
0.70-1.20
|
1.00
|
1.00
|
0.50
|
0.010
|
0.50
|
0.015
|
3. Inconel X-750 Alloy steel physical properties
Inconel X-750 Alloy steel The melting temperature range 1395-1425 degree.
Inconel X-750 Alloy steel Density : 8.25g/cm3
4. InconelX-750 alloy steel Mechanical properties
|
Product
|
Tensile strength /MPa
|
Yield strength MPa
|
Elongation /%
|
HRC
|
|
Inconel X-750 Alloy steel Strip
|
≤930
|
-
|
≥18
|
-
|
|
≥1105
|
-
|
≥12
|
≥30
|
|
|
≤930
|
≤515
|
≥30
|
-
|
|
|
≤930
|
≤515
|
≥35
|
-
|
|
|
Inconel X-750 Alloy hot rooled steel plate
|
≥1170
|
≥795
|
≥18
|
≥32
|
|
Inconel X-750 Alloy steel tube
|
≤965
|
≤550
|
≥35
|
-
|
|
≥1170
|
≥790
|
≥15
|
-
|
Product
- Nickle alloys & Super alloys
- Stainless steel & Heat resistant steel
- Carbon steel
- Low alloy high strength steel
- High strength steel
- Boiler steel plate
- Shipbuilding steel plate
- Bridge structural steel
- Weathering steel
- Wear resistant steel
- Pipeline steel
- High carbon steel
- Alloy steel
- CQ/DQ/DDQ/CSS/HSS Grade steel
- Hot rolled steel coil
- Cold rolled steel coil
- Pickled & oiled steel coil
- Electrical steel
- Galvanized and prepainted steel
- Shipbuilding angle steel bar
- Shipbuilding bulb flat bar
- Shipbuilding L shape bars
About Us
Manufacture